MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wacker Belsil® REG 1100 Crosspolymer
Categories: Fluid; Polymer

Material Notes: BELSIL® REG 1100 resin elastomer gel is a nonemulsifying silicone copolymer network blended with a non-volatile, low viscosity dimethicone. It is a transparent gel, which provides a very pleasant sensory property both during application and afterwards. BELSIL® REG 1100 can act as a thickener in formulations while delivering a smooth application. It exhibits shear-thinning behavior. This attribute allows for formulation of cosmetic products that spread easily during application and facilitates the incorporation of pigments into a formulation.

Special features: BELSIL® REG 1100 is easy to distribute on skin and gives a unique silky feel. The incorporation of a silicone resin into the elastomer structure of BELSIL® REG 1100 provides a long lasting non-tacky film, which improves the water and transfer resistance of formulations. BELSIL® REG 1100 acts as a carrier for fragrances and allows a slow release of the fragrance.

Application: BELSIL® REG 1100 is added to the oil or silicone phase of a formulation or most preferably to an already formed emulsion. The product should be dispersed to yield optimum results, but short times of stirring are sufficient. When BELSIL® REG 1100 is diluted with solvents, the viscosity of the product decreases significantly and hence can be easily adjusted. BELSIL® REG 1100 is used as an ingredient for various skin care, color cosmetic and hair care products. It provides a substantive hydrophobic film, making it ideal for use in sun care formulations. In lipsticks and foundations, it improves transfer resistance. BELSIL® REG 1100 also imparts a cushiony feel to moisturizing creams, sunscreens lotions, eye gels, foundations, concealers and BB creams. BELSIL® REG 1100 can be used to thicken the oil phase of emulsions or anhydrous cosmetic formulations. In pressed powder cosmetics it acts as binder. Other typical applications of BELSIL® REG 1100 include mascara, cleansing products, styling products, conditioners, deodorants and much more.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.930 g/cc0.0336 lb/in³EN/ISO 1183
Solids Content 100 %100 %
Viscosity 75000 - 125000 cP75000 - 125000 cPDIN 53016
 
Thermal PropertiesMetricEnglishComments
Flash Point >= 140 °C>= 284 °FISO 2592
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %"Transparent" but manufacturer does not quantify.
 
Descriptive Properties
Appearancetransparent gel
Content (%)16Elastomer
SolubilityBELSIL® DM 0.65miscible, slightly turbid; 1:1 ratio
 BELSIL® DM 0.65miscible, slightly turbid; 9 (liquid):1 (REG 1100) ratio
 BELSIL® DM 1 Plusmiscible, slightly turbid; 1:1 ratio
 BELSIL® DM 1 Plusmiscible, slightly turbid; 9 (liquid):1 (REG 1100) ratio
 BELSIL® DM 10- DM 500000miscible clear turbid; 9 (liquid):1 (REG 1100) ratio
 BELSIL® DM 10- DM 500000miscible, slightly turbid; 1:1 ratio
 BELSIL® DM 5miscible clear turbid; 9 (liquid):1 (REG 1100) ratio
 BELSIL® DM 5miscible, slightly turbid; 1:1 ratio
 BELSIL® PDM 20miscible, slightly turbid; 1:1 ratio
 BELSIL® PDM 20miscible, slightly turbid; 9 (liquid):1 (REG 1100) ratio
 C12-15 alkyl benzoatesmiscible, turbid; 1:1 ratio
 C12-15 alkyl benzoatesnot miscible; 9 (liquid):1 (REG 1100) ratio
 C9-13 isoparaffinmiscible clear; 9 (liquid):1 (REG 1100) ratio
 C9-13 isoparaffinmiscible, clear; 1:1 ratio
 Capriylic/Capric triglyceridesmiscible, turbid; 1:1 ratio
 Capriylic/Capric triglyceridesnot miscible; 9 (liquid):1 (REG 1100) ratio
 Castor oilnot miscible; 1:1 ratio
 Castor oilnot miscible; 9 (liquid):1 (REG 1100) ratio
 Decyl oleatemiscible, turbid; 1:1 ratio
 Decyl oleatenot miscible; 9 (liquid):1 (REG 1100) ratio
 Dicapryly Ethermiscible, clear; 1:1 ratio
 Dicapryly Ethermiscible, slightly turbid; 9 (liquid):1 (REG 1100) ratio
 Diethylhexyl carbonatemiscible, clear; 1:1 ratio
 Diethylhexyl carbonatemiscible, slightly turbid; 9 (liquid):1 (REG 1100) ratio
 Diisobutyl adipatemiscible, slightly turbid; 1:1 ratio
 Diisobutyl adipatenot miscible; 9 (liquid):1 (REG 1100) ratio
 Ethanolnot miscible; 1:1 ratio
 Ethanolnot miscible; 9 (liquid):1 (REG 1100) ratio
 Ethyhexyl Stearatemiscible, turbid; 1:1 ratio
 Ethyhexyl Stearatenot miscible; 9 (liquid):1 (REG 1100) ratio
 Ethylhexyl Salicylatenot miscible; 1:1 ratio
 Ethylhexyl Salicylatenot miscible; 9 (liquid):1 (REG 1100) ratio
 Glycerolnot miscible; 1:1 ratio
 Glycerolnot miscible; 9 (liquid):1 (REG 1100) ratio
 Hydrogenated Polydecenemiscible, turbid; 1:1 ratio
 Hydrogenated Polydecenenot miscible; 9 (liquid):1 (REG 1100) ratio
 Isopropanolmiscible, slightly turbid; 1:1 ratio
 Isopropanolnot miscible; 9 (liquid):1 (REG 1100) ratio
 Isopropyl myristatemiscible, clear; 1:1 ratio
 Isopropyl myristatemiscible, slightly turbid; 9 (liquid):1 (REG 1100) ratio
 Lanolin oilmiscible, turbid; 1:1 ratio
 Lanolin oilnot miscible; 9 (liquid):1 (REG 1100) ratio
 Mineral oilmiscible, turbid; 1:1 ratio
 Mineral oilnot miscible; 9 (liquid):1 (REG 1100) ratio
 Oleyl oleatenot miscible; 1:1 ratio
 Oleyl oleatenot miscible; 9 (liquid):1 (REG 1100) ratio
 Olive oilnot miscible; 1:1 ratio
 Olive oilnot miscible; 9 (liquid):1 (REG 1100) ratio
 Polyglyceryl 2-Sesquiisosteratenot miscible; 1:1 ratio
 Polyglyceryl 2-Sesquiisosteratenot miscible; 9 (liquid):1 (REG 1100) ratio
 PPG-2 Myristyl Ether Propionatemiscible, turbid; 1:1 ratio
 PPG-2 Myristyl Ether Propionatenot miscible; 9 (liquid):1 (REG 1100) ratio
 Propylene glycolnot miscible; 1:1 ratio
 Propylene glycolnot miscible; 9 (liquid):1 (REG 1100) ratio
 Sorbitan Trioleatenot miscible; 1:1 ratio
 Sorbitan Trioleatenot miscible; 9 (liquid):1 (REG 1100) ratio
 Waternot miscible; 1:1 ratio
 Waternot miscible; 9 (liquid):1 (REG 1100) ratio
 Wheat germ oilnot miscible; 1:1 ratio
 Wheat germ oilnot miscible; 9 (liquid):1 (REG 1100) ratio

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWACK9038 / 204567

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.