MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Covestro DESMODUR® LU-D90 + MOCA Polyurethane, TDI-Ester
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes:

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.19 g/cc1.19 g/ccDESMODUR® LU-D90
 1.25 g/cc1.25 g/ccMOCA
Viscosity 750 cP750 cP
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9090DIN 53505
 90
@Temperature 80.0 °C
90
@Temperature 176 °F
DIN 53505
 95
@Temperature -5.00 °C
95
@Temperature 23.0 °F
DIN 53505
Tensile Strength at Break 56.0 MPa8120 psiDIN 53504
Tensile Stress at Strain 4.30 MPa
@Strain 10 %
624 psi
@Strain 10 %
DIN 53504
Elongation at Break 600 %600 %DIN 53504
100% Modulus 8.00 MPa
@Strain 100 %
1160 psi
@Strain 100 %
DIN 53504
200% Modulus 10.5 MPa
@Strain 200 %
1520 psi
@Strain 200 %
DIN 53504
300% Modulus 14.8 MPa
@Strain 300 %
2150 psi
@Strain 300 %
DIN 53504
Resilience 3131[%]; DIN 53512
Tear Strength 82.0 kN/m468 pliwith nick; ISO 34-1
 119 kN/m679 pliwithout nick; ISO 34-1
Abrasion 3535[mm3]; ISO 4649
Compression Set 32 %
@Temperature 70.0 °C,
Time 79200 sec
32 %
@Temperature 158 °F,
Time 22.0 hour
ISO 815-1
 
Processing PropertiesMetricEnglishComments
Processing Temperature 80.0 °C176 °FDESMODUR® LU-D90
 120 °C248 °FMOCA
Mold Temperature 100 °C212 °F
Pot Life 5.50 min5.50 min
 
Descriptive Properties
AppearanceliquidMOCA
 solidDESMODUR® LU-D90
Content100DESMODUR® LU-D90
 12.5MOCA
 3.95-4.35%NCO

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro DESMODUR® LU-D80 + MOCA Polyurethane, TDI-Ester
Covestro DESMODUR® 0363 + BAYTEC® XL 0328 + BAYTEC® 0354 + BAYTEC® 0340 92A Polyurethane, MDI PPG
Covestro DESMODUR® 0363 + BAYTEC® XL 0328 + BAYTEC® 0354 + BAYTEC® 0340 90A Polyurethane, MDI PPG
Covestro DESMODUR® 0363 + BAYTEC® XL 0328 + BAYTEC® 0354 + BAYTEC® 0340 85A Polyurethane, MDI PPG
Covestro DESMODUR® 0363 + BAYTEC® XL 0328 + BAYTEC® 0354 + BAYTEC® 0340 80A Polyurethane, MDI PPG

PCOVEST0370 / 202153

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.