MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Chromium Copper, UNS C18200, TB00 Temper, Flat Products & Rod
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Precipitation Hardened

Fabrication Properties: Excellent Suitability – Capacity for Being Cold Worked; Good Suitability – Soldering, Brazing, Gas Shielded Arc Welding, Capacity for Being Hot Formed; Fair Suitability – Butt Weld

Common Fabrication Processes: Bending; Cold working; Drawing; Extruding; Forging; Heading; Hot working; Impacting; Rolling; Swaging

Typical uses: Pencil-type & Light Soldering Guns: Tips, Rod Extensions; Arcing and Bridging Parts; Cable; Circuit Breaker Parts; Connectors; Contacts; Electric Motor and Generator Components; Electrical Conductors Requiring Greater Strength than Copper; Electrical Connectors; Electron Tube Grid Side Rods; Parts for Electronic Devices; Semi Conductor Bases; Switch Contacts; Switch Gears; Thermal Conductors Requiring Greater Strength than Copper; Wire, High Temperature; Current Carrying Shafts and Arms; Electrode Holder Jaws; Flash Welding Electrodes; Heat Sinks; Molds; Plastic Mold Components; Resistance Welding Machine Electrodes; Seam Welding Wheels; Spot Welding Tips; Structural Parts; Wear Plates on Heavy Equipment

Applicable Specifications: Bar – MILITARY MIL-C-19311; Forgings – MILITARY MIL-C-19311; Rod – MILITARY MIL-C-19311; Strip – MILITARY MIL-C-19311; Wire – Soft ASTM F9

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.89 g/cc0.321 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength  234 MPa
@Thickness 1.02 mm
34000 psi
@Thickness 0.0400 in
 310 MPa
@Thickness 12.7 mm
45000 psi
@Thickness 0.500 in
Tensile Strength, Yield  96.5 MPa
@Thickness 12.7 mm
14000 psi
@Thickness 0.500 in
0.5% Ext
 131 MPa
@Thickness 1.02 mm
19000 psi
@Thickness 0.0400 in
0.5% Ext
Elongation at Break  40 %
@Thickness 12.7 mm
40 %
@Thickness 0.500 in
 40 %
@Thickness 1.02 mm
40 %
@Thickness 0.0400 in
Tensile Modulus 117 GPa17000 ksi
Modulus of Rigidity 49.6 GPa7200 ksi
Machinability 40 %40 %
Forgeability 80 %80 %
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000220 ohm-cm0.00000220 ohm-cm80% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.6 µm/m-°C
@Temperature 20.0 - 100 °C
9.80 µin/in-°F
@Temperature 68.0 - 212 °F
Specific Heat Capacity 0.385 J/g-°C0.0920 BTU/lb-°F
Thermal Conductivity 26.9 W/m-K187 BTU-in/hr-ft²-°F
Melting Point 1070 - 1075 °C1958 - 1967 °F
Solidus 1070 °C1958 °F
Liquidus 1075 °C1967 °F
 
Processing PropertiesMetricEnglishComments
Solution Temperature 1000 - 1030 °C
@Time 15.0 sec
1832 - 1886 °F
@Time 0.00417 hour
Air
Hot-Working Temperature 816 - 927 °C1500 - 1700 °F
Precipitation Temperature 460 °C860 °FAir
 
Component Elements PropertiesMetricEnglishComments
Chromium, Cr 0.60 - 1.2 %0.60 - 1.2 %
Copper, Cu 98.6 - 99.4 %98.6 - 99.4 %As Balance
Iron, Fe <= 0.10 %<= 0.10 %
Lead, Pb <= 0.050 %<= 0.050 %
Silicon, Si <= 0.10 %<= 0.10 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC18200x4 / 292845

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.