Halogen-free, thermoplastic, highly flame retardant insulation and sheathing compound for low and medium voltage cables Compound class: Insulation/Sheathing Compound category: TP Flame retardant: ATH Standards: DIN EN 50363-7 TI6, TI7; BS 7655 LTS 1 & LTS 3; IEC 60092-360 SHF 1; DIN EN 50363-8 TM7; VDE 0207 part 24 HM 2; DIN VDE 0281 part14 TM 7; VDE 0250 part 215 HM 5 Typical applications: Halogen-free, low smoke, thermoplastic, highly flame retardant compound for the sheathing of low and medium voltage cables in General Installations applications. This compound features a high line speed and good processability. Features: Flame retardant; Halogen-free; Low smoke Information provided by Melos |