MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ExxonMobil Exxon™ Butyl 065S Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Low Mooney grade. White to light amber bales.

Butyl rubber is a copolymer of isobutylene and a small amount of isoprene, providing for a highly saturated backbone. The primary properties of butyl rubber are excellent air-barrier performance, good flex fatigue and vibration damping. From inner tubes to curing bladders, butyl properties are valued across a range of rubber products. Benefits: Low permeability to air, gases and moisture, Vibration damping, Low glass transition temperature, Low modulus elastomer, Low compression set, Resistance to aging and to weathering from atmospheric exposure, Wide vulcanization versatility, Fast cure rates,  Processing safety: no nitrosamines or nitrosamines precursors,  Broad range of durometer and tensile strength properties, Low filler content for specific gravity, cost-effective compounding.  Exxon butyl rubber is a copolymer of isobutylene and isoprene.

Information provided by ExxonMobil.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.920 g/cc0.0332 lb/in³
Mooney Viscosity 28 - 36
@Temperature 125 °C
28 - 36
@Temperature 257 °F
ML 1+8. MV 200 or equivalent; ASTM D1646
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 0.30 %<= 0.30 %ExxonMobil Method
 
Descriptive Properties
Antioxidant (non-staining)0.03min wt%. Non-staining. ExxonMobil Method
Unsaturation0.85 - 1.25mol %. ExxonMobil Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Butyl Rubber (IIR, CIIR, BIIR)

PEX98802 / 238187

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.