MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Akrochem Akrochem Antioxidant BLS-25
Categories: Other Engineering Material

Material Notes: Product Description: Akrochem Antioxidant BLS-25 is a reaction product of acetone and diphenylamine. Akrochem Antioxidant BLS-25 offers protection against flex-cracking, heat and oxidation to natural and synthetic elastomers such as NR, CR, NBR, SBR, BR and EPDM. Dark brown discoloration in compounds when exposed to light and contact staining to light colored rubber articles should be a concern. Akrochem Antioxidant BLS-25 has minimal effect on cure rate and cure state and is non-blooming after cure but can migrate during cure. The antioxidant is suitable for peroxide cure with little or no effect. Akrochem Antioxidant BLS-25 is insoluble in water and gasoline but soluble in acetone, ethylene dichloride and benzene.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/cc
 
Descriptive Properties
AppearanceDark Brown Viscous Liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAKZCH520 / 315438

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.