MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Epoxy Technology EPO-TEK® H35-175MP Electrically Conductive, Silver Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy, Electrically Conductive

Material Notes: Product Description: EPO-TEK® H35-175MP is a single component, silver-filled, electrically conductive epoxy designed for semiconductor die attach applications found in hybrids, JEDEC, and opto-electronic packaging. Low viscosity version of EPO-TEK® H31.

Advantages & Application Notes:

  • Exhibits a smooth, flowing consistency that is adaptable to conventional processing methods such as dispensing and screen printing. See Technical Paper #43 from our website link for hints and best practices for high speed auger screw dispensing
  • Performs exceptionally well as a die attach for small chips such as GaAs, LEDs and diodes.
  • Capable of resisting 260°C green reflow process, low outgassing in hermetic lid-seal processes near 300°C, and organic burn-in up to 150°C/1000 hours storage.
  • Certified to MIL-STD 883/Test Method 5011 –yields low levels of water extractable monovalent ions such as Chlorides.
  • Passes NASA low outgassing standard ASTM E595 with proper cure
  • Capable of JEDEC Level II die-attach packaging on die-paddles and lead-frames.
  • Widely used epoxy; popular choice for silver-filled epoxies; opto-packaging, hybrids, and many types of substrates including kovar, ceramic and BT.
  • Available in many different viscosity ranges

Information Provided by Epoxy Technology

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 3.07 g/cc
Particle Size <= 20 µm
Viscosity 22000 - 28000 cP
@Temperature 23.0 °C
10 rpm
 
Chemical PropertiesOriginal ValueComments
Ionic Impurities - Na (Sodium) <= 50 ppm
Ionic Impurities - K (Potassium) <= 50 ppm
Ionic Impurities - Cl (Chloride) <= 200 ppm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 83
Tensile Modulus 1.107e+6 psiStorage
Shear Strength >= 2000 psiLap
 >= 3400 psiDie
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 0.00050 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 31.0 µm/m-°CBelow Tg
 97.0 µm/m-°CAbove Tg
Thermal Conductivity 1.50 W/m-K
Maximum Service Temperature, Air 200 °CContinuous
 300 °CIntermittent
Minimum Service Temperature, Air -55.0 °CContinuous
 -55.0 °CIntermittent
Glass Transition Temp, Tg >= 100 °CDynamic Cure 20—300°C /ISO 25 Min; Ramp -10—200°C @ 20°C/Min
Decomposition Temperature 372 °CDegradation Temperature
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 hour
@Temperature 180 °C
Minimum Bond Line
 1.50 hour
@Temperature 165 °C
Minimum Bond Line
Pot Life 40320 min
Shelf Life 12.0 Month
@Temperature -40.0 °C
 
Descriptive Properties
ColorBright silver
ConsistencySmooth thixotropic paste
Ionic Impurities NH439 ppm
Number of ComponentsSingle
Thixotropic Index4
Weight Loss0.13%200°C
 0.14%250°C
 0.28%300°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Epoxy Technology EPO-TEK® E3001-HV Electrically Conductive, Silver Epoxy
Epoxy Technology EPO-TEK® H20E-175 Electrically Conductive, Silver Epoxy
Epoxy Technology EPO-TEK® E2116 Electrically Conductive, Silver Epoxy
Epoxy Technology EPO-TEK® H20E Electrically Conductive, Silver Epoxy
Epoxy Technology EPO-TEK® E4110 Electrically Conductive, Silver Epoxy

PPOXYT045 / 141084

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.