MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials Kalrez® 8575 FFKM Perfluoroelastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: Kalrez® Sahara™ 8575 is specially formulated for improved performance in etching, ashing and stripping processes, offers lower cost of ownership with reduced contamination and longer seal life. This white perfluoroelastomer compound utilizes a new proprietary polymer and crosslinking system. It offers reduced weight loss, particle generation and outgassing, as well as improved elastic recovery properties. Kalrez® Sahara™ 8575 exhibits excellent resistance to both oxygen and fluorine plasma as well as chlorinated cleaning gasses (e.g., CIF3). It has excellent vacuum and long-term sealing performance, good mechanical properties and is well-suited for both static and dynamic sealing applications (e.g., gas inlets, chamber lids, slit valve doors, etc.). A maximum continuous service temperature of 300°C is suggested. Ultrapure post-cleaning and packaging is standard for all parts made of Kalrez® Sahara™ 8575.

Information provided by manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.26 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 63ASTM D 2240
Elongation at Break 220 %ASTM D 412
100% Modulus 3.00 MPaASTM D 412
Compression Set 17 %
@Temperature 204 °C,
Time 252000 sec
O-ring (AS568-214); ASTM D 1414
 23 %
@Temperature 204 °C,
Time 252000 sec
Pellet (Type 1); ASTM D 395B
 
Thermal PropertiesOriginal ValueComments
CTE, linear 285 µm/m-°CISO 11359-1/-2
Maximum Service Temperature, Air 300 °CDuPont proprietary test
Minimum Service Temperature, Air -3.00 °CRetraction temperature TR-10; ASTM D 1329
 
Descriptive Properties
ColorWhite
Polymer(FFKM)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Kalrez® 6221 FFKM Perfluoroelastomer
DuPont Mobility and Materials Kalrez® 6375 FFKM Perfluoroelastomer
DuPont Mobility and Materials Kalrez® 4079 FFKM Perfluoroelastomer
DuPont Mobility and Materials Kalrez® 6375UP FFKM Perfluoroelastomer
DuPont Mobility and Materials Kalrez® 6230 FFKM Perfluoroelastomer

PDVD059 / 33878

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.