MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Shandong Dongyue Shenzhou New Material Co DS201 Polyvinylidene Fluoride Powder
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF)

Material Notes: Conformable with: Q/DYS 014-2007

Polyvinylidene fluoride (PVDF) powder (DS201) PVDF is the homopolymer of vinylidene fluoride, which is excellent chemical corrosion-resistant, high temperature resistant, resistant to oxidation and climate, resistant to ultraviolet radiation and high-energy. The using temperature range is -60 to 150°C, and the thermal stability is up to 316°C. Polyvinylidene fluoride (PVDF) powder (DS201) and acrylic resins, additives can be mixed from superior performance baking polyvinylidene fluoride (PVDF) fluorocarbon coating.

Main Applications:

Mainly for high buildings' external decorative coatings, billboards, highway, etc.

Information Provided by Shandong Dongyue Shenzhou New Material Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.75 - 1.77 g/ccStand relative density
Particle Size <= 75 µmScattered Fineness
Melt Flow 0.50 - 4.5 g/10 min
 
Thermal PropertiesOriginal ValueComments
Melting Point 156 - 161 °C
Decomposition Temperature >= 390 °C
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.10 %
 
Descriptive Properties
AppearanceWhite Powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Techmer ES HiFill® TPX-PVDF-03009 C
Westlake Plastics Kynar® CN-F PVDF Polyvinylidene Fluoride (conductive)
Westlake Plastics Kynar® 2850 PVDF Copolymer
Shanghai Ofluorine D-1 PVDF Lithium Ion Battery Binders (DF-2)

PSHEN037 / 104092

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.