MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Avient ECCOH™ 0521-48 Low Smoke Free Of Halogen (LSFOH)  (discontinued **)
Categories: Polymer; Thermoplastic

Material Notes:

ECC0H non-halogenated flame-retardant polyolefin compounds are ideal for applications that require non-corrosive materials such as mass transit, tunnels, and airports. Originally designed to meet European requirements in the transportation industry, these compounds are used for both sheathing and primary insulation. Specially designed for thin wall extrusion wire and cable applications, ECC0H compounds are low smoke and highly flame-retardant, and will not emit corrosive gasses when burned.

Description/Features:

  • Non-Halogenated
  • Low Smoke
  • Flame Retardant

Applications:

  • Thin-wall extrusion applications (Tape, x-web)

Market:

  • Wire & Cable

Processing Method:

  • Extrusion

TENSILE AND ELONGATION VALUES ARE LARGELY DETERMINED BY PROCESSING PARAMETERS OF THE END USER. NOTE: Tensile property data is from extruded tape 3:1 drawdown ratio and .006 in. NOTE: Dielectric Constant is measured on .085" plaque).PolyOne First Choice

Disclaimer: NOTE: Typical Properties of Molded Slab (0.075"); Not to be Construed as Specifications.

Information provided by PolyOne Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.461 g/ccASTM D792
Melt Flow 0.73 g/10 min
@Load 2.16 kg,
Temperature 190 °C
Procedure A - Manual Operation; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 2000 psiType 4 - Flexibles, Break, 20 in/min; ASTM D638
Elongation at Break 450 %Type 4 - Flexibles, 20 in/min; ASTM D638
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.06
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
Oxygen Index 30 %ASTM D2863
 
Descriptive Properties
AppearancePellets/CubesASTM D2090

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient ECCOH™ 5801 Low Smoke Free Of Halogen (LSFOH)
Samyang Triel® 5700 Thermoplastics Polyetherester Elastomer, General Extrusion

PH1PO0028 / 43337

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.