MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Trinseo MAGNUM™ 3504 ABS
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: Product Description: MAGNUM™ 3504 is a general purpose resin and can be used for both injection molding and extrusion applications. This grade combines high impact with medium-high heat resistance. The mass (continuous process) ABS technology ensures an ABS resin that combines excellent processability with a stable light base color that is ideal for self-coloring.
Applications: General purpose extrusion

Availability: Asia Pacific; Europe; Latin America; North America

Features: Good Impact Resistance; Good Processability; Medium Heat Resistance

Uses: General Purpose

Form: Pellets

Processing Method: Injection Molding; Profile Extrusion; Sheet Extrusion

Information provided by Trinseo

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.650 g/cc0.0235 lb/in³ISO 60
Density 1.05 g/cc0.0379 lb/in³ISO 1183
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/inISO 294-4
Melt Flow 5.2 g/10 min
@Load 10.0 kg,
Temperature 220 °C
5.2 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 43.0 MPa6240 psiISO 527-2/50
Elongation at Yield 2.7 %2.7 %ISO 527-2/50
Tensile Modulus 2.14 GPa310 ksiIOS 527-1/1
Flexural Strength 65.0 MPa9430 psiISO 178
Flexural Modulus 2.05 GPa297 ksiISO 178
Charpy Impact, Notched 2.31 J/cm²11.0 ft-lb/in²Injection Molded; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 101 °C214 °FUnannealed; ISO 75-2/A
Vicat Softening Point 102 °C216 °FISO 306/B50
Flammability, UL94  HB
@Thickness 1.52 mm
HB
@Thickness 0.0600 in
 HB
@Thickness 3.05 mm
HB
@Thickness 0.120 in
 
Processing PropertiesMetricEnglishComments
Drying Temperature 80.0 - 90.0 °C176 - 194 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
 
Descriptive Properties
Carbon Emission30 µg/gVDA 277
Fogging98ISO 6452

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTRINSE1537 / 312230

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.