Grade MC320LE is a fine weave bleached cotton phenolic composite that has excellent machining characteristics and low moisture absorption. Applications include marine applications, terminal boards and parts requiring medium strength and excellent electrical characteristics. MC320LE meets or exceeds the requirements of MIL-I-24768/13.Information provided by Norplex-Micarta |
Cotton, Phenolic, Micarta, MIL-I-24768/13-FBE, ASTM D709 Type II Grade LE, NEMA LE |