MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

SCG Chemicals EL-Pro™ P602F Polypropylene Film Resin
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Key Characteristics:
  • Excellent optical properties
  • High productivity

Recommended Applications:

  • Water quenched blown film for food and apparel packaging
  • Can be blended with P600 for excellent clarity

Information provided by SCG Chemicals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.910 g/cc0.910 g/ccASTM D1505
Thickness 25.0 microns0.984 mil
Melt Flow 10 g/10 min
@Load 2.16 kg,
Temperature 230 °C
10 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 28.0 MPa4060 psiASTM D882
Film Tensile Strength at Yield, TD 20.0 MPa2900 psiASTM D882
Film Elongation at Break, MD 850 %850 %ASTM D882
Film Elongation at Break, TD 770 %770 %ASTM D882
Flexural Modulus 1.67 GPa242 ksiASTM D790
Secant Modulus, MD 0.690 GPa100 ksiASTM D882
Secant Modulus, TD 0.540 GPa78.3 ksiASTM D882
Izod Impact, Notched 0.245 J/cm0.459 ft-lb/inASTM D256
Film Tensile Strength at Break, MD 27.0 MPa3920 psiASTM D882
Film Tensile Strength at Break, TD 26.0 MPa3770 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 160 °C320 °FASTM D2117
Deflection Temperature at 0.46 MPa (66 psi) 110 °C230 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C140 °FASTM D648
Vicat Softening Point 155 °C311 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 8.0 %8.0 %ASTM D1003
Gloss 75 %75 %ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSCGC951 / 120705

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.