Formolene FORMAX® L91904B is a linear low density, high molecular weight hexene copolymer resin that is tailored specifically for geomembrane applications. The resin provides outstanding ESCR properties, broad fusion range, excellent melt strength and good processability.Information provided by Formosa Plastics Corporation, U.S.A. |