MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Henkel Loctite® Stycast® U 2500 TEM Two-Component Polyurethane Encapsulant
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Loctite Stycast U 2500 TEM provides the following product characteristics:
  • Low viscosity
  • Flexible
  • Excellent wetting properties

Cure: Room Temperature or Heat Cure

Application: Encapsulant

Typical Assembly Applications: Transformers, PCB's and other insulating applications

Loctite Stycast U 2500 TEM flexible polyurethane encapsulant is formulated to have low viscosity and excellent wetting properties allowing complete impregnation of either small slightly wound coils or large castings.

Information provided by Henkel.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.23 g/cc0.0444 lb/in³Part B
 1.50 g/cc0.0542 lb/in³Part A
Moisture Absorption 0.800 %
@Time 86400 sec
0.800 %
@Time 24.0 hour
Viscosity 5.0 cP5.0 cPPart B
 6000 cP6000 cPMixed
 12500 cP12500 cPPart A
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7575
Tensile Strength 3.50 MPa508 psi
Elongation at Break 70 %70 %
Modulus of Elasticity 0.00700 GPa1.02 ksi
Adhesive Bond Strength 2.50 MPa363 psiTensile Lap Shear Strength, Al to Al
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 5.00e+11 ohm-cm5.00e+11 ohm-cm500 Volts
Surface Resistance 1.00e+14 ohm1.00e+14 ohm
Dielectric Constant 6.0
@Frequency 1e+6 Hz
6.0
@Frequency 1e+6 Hz
Dissipation Factor 0.060
@Frequency 1e+6 Hz
0.060
@Frequency 1e+6 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 175 µm/m-°C97.2 µin/in-°F
Thermal Conductivity 0.600 W/m-K4.16 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 125 °C257 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
Glass Transition Temp, Tg -68.0 °C-90.4 °FTMA
 
Processing PropertiesMetricEnglishComments
Cure Time  240 min
@Temperature 60.0 °C
4.00 hour
@Temperature 140 °F
Alternate, A post cure of 2 hours @ 100 to 120°C is recommended.
 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
Recommended, Post cure of 2 hours @ 100 to 120°C is recommended.
Pot Life 45.0 min45.0 min
Shelf Life 6.00 Month
@Temperature 18.0 - 25.0 °C
6.00 Month
@Temperature 64.4 - 77.0 °F
 
Descriptive Properties
AppearanceAmberPart B
 BlackPart A
Mix Ratio, by Volume100 : 8.5Part A : Part B
Mix Ratio, by Weight100 : 7Part A : Part B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHENK7963 / 255447

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.