MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Novatec Novablend® 4780 PVC  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Rigid Grade

Material Notes: Clear Pellets

Description: Novablend® 4780 is a general purpose, high impact, rigid, PVC, extrusion blow molding compound in pellet form. The formulation is designed to provide good processing characteristics in high output wheel machines, high impact, and excellent thermal stability. This formulation is also designed to assist in light weighting of bottles in order to comply with source reduction. Bottles produced with this compound have high impact with excellent gloss and clarity.

Applications: Bottles made with Novablend® 4780 are suitable for a variety of toiletries and cosmetic applications, including shampoo, hair rinses, creams, and other personal care products.

Information supplied by the manufacturer.

PolyOne (Avient) acquired the Novatec polymer resin product line. This grade is not a part of their current product line

Key Words: General purpose, high impact, rigid PVC compound
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.32 - 1.36 g/cc0.0477 - 0.0491 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 40.7 MPa5900 psiASTM D638
Modulus of Elasticity 2.62 GPa380 ksiASTM D638
Flexural Yield Strength 71.0 MPa10300 psiASTM D790
Flexural Modulus 2.41 GPa350 ksiASTM D790
Izod Impact, Notched 8.50 J/cm15.9 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C158 °FASTM D648

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema Nakan® RMA 705 N PVC, Rigid Injection Molding Grade
Arkema Nakan® RMS 501 L PVC, Rigid Injection Molding Grade
Colorite Polymers 2007F Rigid PVC
Geon® Performance Solutions 81520 Polyvinyl Chloride, Rigid
Karina 802-18/462-C-ERB Gray PVC Compound

PNV023 / 55484

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.