Product Overview: Mold Max™ XLS™ II is a Shore 30A tin-catalyzed silicone rubber that exhibits very low long-term shrinkage. XLS™ II molds last longer than other silicones in production when casting chemically harsh resins such as epoxies and polyesters as well as urethane foams. Mix ratio is 100A:10B by weight. Pot life is 40 minutes and cure time is 24 hours at room temperature. Mold Max™ XLS™ II silicone will reproduce the finest detail and is suitable for a variety of industrial and art related applications including making production molds for, reproducing prototypes, furniture, sculpture and architectural elements. Mold Max™ XLS™ II can be thickened with THI-VEX™ additive for brush-on applications. Important; you must weigh Part A & B components using a gram scale to be successful with Mold Max™ XLS II. Vacuum degassing mixed material using a vacuum pump and chamber to remove entrapped air is recommended.Information provided by Reynolds Advanced Materials |