Flocklok® P13 is a moisture curing, flexible polyurethane adhesive used for automotive weatherstrip sealing profiles to flock. This adhesive will adhere polyester or polyamide flock to a variety of elastomers including EPDM, NR, CR, and SBR.All information provided by Lord. |