MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

AlphaGary Megolon™ S800 Low Smoke Halogen Free
Categories: Polymer; Thermoplastic

Material Notes: A thermoplastic, halogen free, fire retardant high speed cable sheathing compound for general purpose applications. This product exhibits excellent processing characteristics including the ability to extrude at very high speeds and has been specifically designed to allow cable manufacturers to maximize volumetric output and efficiency. Application examples include Telecommunications Cables / Data Cables.

Alphagary is part of Orbia.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 12.0 MPa1740 psi
Elongation at Break 150 %150 %IEC60811-1-1
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 174 °C345 °FTemperature Index
Oxygen Index 30 %30 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AlphaGary Megolon™ S540E Low Smoke Halogen Free
AlphaGary Megolon™ S500 Low Smoke Halogen Free
AlphaGary Megolon™ FB119 Low Smoke Halogen Free
AlphaGary Smokeguard™ LS III 1091 A1 Low Smoke Polyvinyl Chloride
Covestro Desmopan® 453 Urethane Thermoplastic Elastomer

PGARY9822 / 140608

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.