MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Epsan Eplamid 66 GX0 30 NC Q1C0D001 Polyamide 66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass Fiber Filled, Flame Retardant

Material Notes: Flame retardant polyamide 66 reinforced with 30% of glass fiber, heat stabilized for injection molding. Halogen and red phosphorous free flame retardant grade, RoHs conform, UL94 V0 and glow-wire at 960°C rated, combines excellent all around mechanical properties.

Information provided by Epsan Plastik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.43 g/ccISO 1183
Linear Mold Shrinkage 0.0030 cm/cmParallel; ISO 294-4
 0.0050 cm/cmNormal; ISO 294-4
Ash 30 %ISO 3451-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Stress 140 MPaISO 527-2
Elongation at Break 2.0 %ISO 527-2
Tensile Modulus 10000 MPaISO 527-2
Flexural Strength 240 MPaISO 178
Flexural Modulus 8900 MPaISO 178
Izod Impact, Notched (ISO) 9.00 kJ/m²ISO 180/1A
Charpy Impact, Notched 10.0 kJ/m²ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 260 °CISO 3146
Flammability, UL94 V-0
@Thickness 1.60 mm
EN 60695-11-10
Glow Wire Ignition Temperature 750 °C
@Thickness 2.00 mm
EN 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 2.00 mm
EN 60695-2-12
 
Processing PropertiesOriginal ValueComments
Processing Temperature 280 °CRecommended Injection Molding Temperature
Drying Temperature 80.0 °CAverage Drying Time is 2-4 hrs
Moisture Content 0.20 %ISO 15512

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEPSAN061 / 186375

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.