MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

SABIC LNP™ STAT-KON™ Compound QD000I Polyamide 610 (Nylon 610)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 610 (PA610)

Material Notes: LNP STAT-KON QD000I compound is based on Nylon 6/10 resin containing conductive carbon powder. Added features of this grade include: Electrically Conductive, High Impact.

Features: High Impact Resistance,Electrically Conductive

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.11 g/cc0.0401 lb/in³ASTM D792
Moisture Absorption 0.120 - 0.200 %0.120 - 0.200 %Injection Molding
 0.280 %0.280 %23°C/50% RH/24 hrs; ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 31.0 MPa4500 psiASTM D638
Elongation at Break 52.7 %52.7 %ASTM D638
Flexural Strength 54.0 MPa7830 psiASTM D790
Flexural Modulus 1.72 GPa249 ksiASTM D790
Izod Impact Notched 603 J445 ft-lbASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 100 - 10000 ohm-cm100 - 10000 ohm-cmASTM D257
Surface Resistance 100 - 10000 ohm100 - 10000 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 117 µm/m-°C
@Temperature -40.0 - 40.0 °C
65.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
CTE, linear, Transverse to Flow 117 µm/m-°C
@Temperature -40.0 - 40.0 °C
65.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
@Thickness 3.20 mm
131 °F
@Thickness 0.126 in
unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Zone 2 260 - 270 °C500 - 518 °F
Zone 3 270 - 280 °C518 - 536 °F
Melt Temperature 270 - 275 °C518 - 527 °FInjection Molding
Mold Temperature 80.0 - 95.0 °C176 - 203 °F
Drying Temperature 80.0 °C176 °FInjection Molding
Dry Time 4.00 hour4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa29.0 - 43.5 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81349 / 289296

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.