MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

SABIC XENOY™ 1102 PC+PBT (Asia)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced

Material Notes: Unreinforced PC/polyester alloy. Excellent low temperatue impact/chemical resistance to automotive fluids.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.19 g/cc1.19 g/ccASTM D792
 1.20 g/cc1.20 g/ccASTM D792
Density 1.19 g/cc0.0430 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0080 - 0.010 cm/cm
@Thickness 3.20 mm
0.0080 - 0.010 in/in
@Thickness 0.126 in
SABIC method
Linear Mold Shrinkage, Transverse 0.0080 - 0.010 cm/cm
@Thickness 3.20 mm
0.0080 - 0.010 in/in
@Thickness 0.126 in
SABIC method
Melt Flow 6.0 g/10 min
@Load 2.16 kg,
Temperature 250 °C
6.0 g/10 min
@Load 4.76 lb,
Temperature 482 °F
cm³/10 min; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 45.0 MPa6530 psi50 mm/min; ISO 527
Tensile Strength, Yield 50.0 MPa7250 psi50 mm/min; ISO 527
 54.0 MPa7830 psi50 mm/min; ASTM D638
Elongation at Break 115 %115 %50 mm/min; ISO 527
 150 %150 %50 mm/min; ASTM D638
Elongation at Yield 4.5 %4.5 %50 mm/min; ISO 527
Flexural Yield Strength 72.0 MPa10400 psi2 mm/min; ISO 178
 82.0 MPa11900 psi1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 1.87 GPa271 ksi2 mm/min; ISO 178
 1.96 GPa284 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 8.00 J/cm15.0 ft-lb/inASTM D256
 6.40 J/cm
@Temperature -30.0 °C
12.0 ft-lb/in
@Temperature -22.0 °F
ASTM D256
 6.90 J/cm
@Temperature 0.000 °C
12.9 ft-lb/in
@Temperature 32.0 °F
ASTM D256
Izod Impact, Notched (ISO) 54.0 kJ/m²25.7 ft-lb/in²80*10*4; ISO 180/1A
 44.0 kJ/m²
@Temperature -30.0 °C
20.9 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
 52.0 kJ/m²
@Temperature 0.000 °C
24.7 ft-lb/in²
@Temperature 32.0 °F
80*10*4; ISO 180/1A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 110 °C
@Thickness 6.40 mm
230 °F
@Thickness 0.252 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °C174 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 90.0 °C
@Thickness 6.40 mm
194 °F
@Thickness 0.252 in
unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 255 - 270 °C491 - 518 °FInjection Molding
Zone 1 245 - 265 °C473 - 509 °F
Zone 2 250 - 270 °C482 - 518 °F
Zone 3 255 - 275 °C491 - 527 °F
Melt Temperature 260 - 275 °C500 - 527 °F
Mold Temperature 65.0 - 90.0 °C149 - 194 °F
Drying Temperature 110 °C230 °FInjection Molding
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hourInjection Molding
 8.00 hour8.00 hourCumulative; Injection Molding
Moisture Content 0.020 %0.020 %
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 50 - 80 %50 - 80 %
Vent Depth 0.00130 - 0.00200 cm0.000512 - 0.000787 in
Screw Speed 50 - 80 rpm50 - 80 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI10806 / 244273

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.