MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Haynes Hastelloy® G-30® alloy, 12.7 mm (1/2 in.) thick plate, GTAW weld 3.2 mm diameter filler wire
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizing acids such as nitric/hydrochloric, nitric/hydrofluoric and sulfuric acids. The resistance of G-30 alloy to the formation of grain boundary precipitates in the heat-affected zone makes it suitable for use in most chemical process applications in the as-welded condition.

HASTELLY G-30 alloy is available in the form of plate, sheet, strip, billet, bar, wire, covered electrodes, pipe and tubing.

Typical Applications:

  • Phosphoric Acid Service
  • Sulfuric Acid Service
  • Nitric Acid Service
  • Nuclear Fuel Reprocessing
  • Nuclear Waste Processing
  • Pickling Operations
  • Petrochemicals
  • Fertilizer Manufacture
  • Pesticide Manufacture
  • Gold Ore Extraction

Heat Treatment: The standard solution heat treatment consists of heating to 2150°F (1177°C) followed by rapid air-cooling or water quenching. Parts which have been hot formed should be solution heat-treated prior to final fabrication or installation.

Forming: G-30 alloy has excellent forming characteristics and cold forming is the preferred method of forming. Because of its good ductility, it can be easily cold-worked. The alloy is generally stiffer than the austenitic stainless steels so more energy is required during cold forming.

Data provided by the manufacturer, Haynes International, Inc.

Key Words: ASME SB622, ASME SB626, ASME SB366, UNS N06030, ASME SB581, ASME SB582, ASME SB619
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.22 g/cc0.297 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 710 MPa103000 psi
 372 MPa
@Temperature 760 °C
54000 psi
@Temperature 1400 °F
 490 MPa
@Temperature 538 °C
71100 psi
@Temperature 1000 °F
Tensile Strength, Yield 393 MPa
@Strain 0.2 %
57000 psi
@Strain 0.2 %
 221 MPa
@Strain 0.2 %,
Temperature 538 °C
32100 psi
@Strain 0.2 %,
Temperature 1000 °F
 221 MPa
@Strain 0.2 %,
Temperature 760 °C
32100 psi
@Strain 0.2 %,
Temperature 1400 °F
Elongation at Break 60 %60 %in 50.8 mm
 33 %
@Temperature 760 °C
33 %
@Temperature 1400 °F
in 50.8 mm
 56 %
@Temperature 538 °C
56 %
@Temperature 1000 °F
in 50.8 mm
Reduction of Area 70 %70 %Fracture in base metal.
 25 %
@Temperature 760 °C
25 %
@Temperature 1400 °F
Fracture in weld metal.
 60 %
@Temperature 538 °C
60 %
@Temperature 1000 °F
Fracture in base metal.
Modulus of Elasticity 202 GPa29300 ksiplate heat treated to 1177°C, rapid quenched
 184 GPa
@Temperature 538 °C
26700 ksi
@Temperature 1000 °F
plate heat treated to 1177°C and rapid quenched
 192 GPa
@Temperature 427 °C
27800 ksi
@Temperature 801 °F
plate heat treated to 1177°C and rapid quenched
 194 GPa
@Temperature 316 °C
28100 ksi
@Temperature 601 °F
plate heat treated to 1177°C and rapid quenched
 196 GPa
@Temperature 204 °C
28400 ksi
@Temperature 399 °F
plate heat treated to 1177°C and rapid quenched
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity  0.000116 ohm-cm
@Temperature 24.0 °C
0.000116 ohm-cm
@Temperature 75.2 °F
 0.000117 ohm-cm
@Temperature 100 °C
0.000117 ohm-cm
@Temperature 212 °F
 0.000119 ohm-cm
@Temperature 200 °C
0.000119 ohm-cm
@Temperature 392 °F
 0.000119 ohm-cm
@Temperature 300 °C
0.000119 ohm-cm
@Temperature 572 °F
 0.000123 ohm-cm
@Temperature 400 °C
0.000123 ohm-cm
@Temperature 752 °F
 0.000124 ohm-cm
@Temperature 500 °C
0.000124 ohm-cm
@Temperature 932 °F
 0.000125 ohm-cm
@Temperature 600 °C
0.000125 ohm-cm
@Temperature 1110 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  14.4 µm/m-°C
@Temperature 30.0 - 316 °C
8.00 µin/in-°F
@Temperature 86.0 - 601 °F
 14.9 µm/m-°C
@Temperature 30.0 - 427 °C
8.28 µin/in-°F
@Temperature 86.0 - 801 °F
 15.5 µm/m-°C
@Temperature 30.0 - 538 °C
8.61 µin/in-°F
@Temperature 86.0 - 1000 °F
 16.0 µm/m-°C
@Temperature 30.0 - 760 °C
8.89 µin/in-°F
@Temperature 86.0 - 1400 °F
 16.0 µm/m-°C
@Temperature 30.0 - 649 °C
8.89 µin/in-°F
@Temperature 86.0 - 1200 °F
Thermal Conductivity  10.2 W/m-K
@Temperature 24.0 °C
70.8 BTU-in/hr-ft²-°F
@Temperature 75.2 °F
 11.9 W/m-K
@Temperature 100 °C
82.6 BTU-in/hr-ft²-°F
@Temperature 212 °F
 14.4 W/m-K
@Temperature 200 °C
99.9 BTU-in/hr-ft²-°F
@Temperature 392 °F
 16.7 W/m-K
@Temperature 300 °C
116 BTU-in/hr-ft²-°F
@Temperature 572 °F
 18.7 W/m-K
@Temperature 400 °C
130 BTU-in/hr-ft²-°F
@Temperature 752 °F
 20.3 W/m-K
@Temperature 500 °C
141 BTU-in/hr-ft²-°F
@Temperature 932 °F
 21.4 W/m-K
@Temperature 600 °C
149 BTU-in/hr-ft²-°F
@Temperature 1110 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.030 %<= 0.030 %
Chromium, Cr 28 - 31.5 %28 - 31.5 %
Cobalt, Co <= 5.0 %<= 5.0 %
Copper, Cu 1.0 - 2.4 %1.0 - 2.4 %
Iron, Fe 13 - 17 %13 - 17 %
Manganese, Mn <= 1.5 %<= 1.5 %
Molybdenum, Mo 4.0 - 6.0 %4.0 - 6.0 %
Nb + Ta 0.30 - 1.5 %0.30 - 1.5 %
Nickel, Ni 43 %43 %As Remainder
Phosphorus, P <= 0.040 %<= 0.040 %
Silicon, Si 0.80 %0.80 %
Sulfur, S <= 0.020 %<= 0.020 %
Tungsten, W 1.5 - 4.0 %1.5 - 4.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Carlson C 625 Nickel-Chromium-Molybdenum Alloy
MetalTek MTEK CW-12MW Cast UNS N30002 Severe Corrosion and Heat Resistant Alloy
MetalTek MTEK N-7M Cast UNS N30007 Severe Corrosion and Heat Resistant Alloy
Chesterton 390 Cutting Oil
Chesterton 389 Synthetic Tapping Compound

NHG3AX / 17288

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.