High density polyethylene. These hexene copolymers are tailored for rotational molding applications that require: - Wide process windows and fair flow
- Long-term UV stabilization
- Excellent impact strength
- Good ESCR
These resins are available in: - Pellet form - HMN TR-942
- 35 US mesh powder - HMN TR-942G
Applications: - Potable water and chemical tanks
- Agricultural equipment
Information provided by Phillips These resins meet the following specifications: - ASTM D4976 - PE 233
- FDA 21 CFR 177.1520(c) 3.2a, use conditions B through H per 21 CFR 176.170(c) Table 2. Single use articles contacting food types I, II, IV-B, VI-A, VI-B, VII-B, and VIII. Repeated use articles contacting all food types defined in 21 CFR 176.170(c) Table 1.
|