MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

DuPont Mobility and Materials Delrin® FG911DP NC010 POM  (discontinued **)
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Homopolymer, Unreinforced

Material Notes: Nucleated Low Viscosity Acetal Homopolymer Developed for Food Contact Applications

Information provided by DuPont; The Delrin product line was sold by DuPont in 2023 but this specific grade was discontinued prior to the sale

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.42 g/cc0.0513 lb/in³ISO 1183
Water Absorption 0.90 %
@Thickness 2.00 mm
0.90 %
@Thickness 0.0787 in
Sim. to ISO 62
Moisture Absorption 0.200 %
@Thickness 2.00 mm
0.200 %
@Thickness 0.0787 in
2mm; Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.019 cm/cm0.019 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.018 cm/cm0.018 in/innormal; ISO 294-4, 2577
Melt Flow 24 g/10 min
@Load 2.16 kg,
Temperature 190 °C
24 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 175 MPa25400 psiH 961/30; DS Sample; ISO 2039-1
Tensile Strength, Yield 75.0 MPa10900 psiISO 527-1/-2
Elongation at Break 20 %20 %Nominal; ISO 527-1/-2
Elongation at Yield 10 %10 %ISO 527-1/-2
Tensile Modulus 3.40 GPa493 ksiISO 527-1/-2
Flexural Yield Strength 90.0 MPa
@Strain 3.5 %
13100 psi
@Strain 3.5 %
ISO 178
Flexural Modulus 3.30 GPa479 ksiISO 178
Poissons Ratio 0.370.37
Charpy Impact Unnotched  15.0 J/cm²
@Temperature -30.0 °C
71.4 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 16.0 J/cm²
@Temperature 23.0 °C
76.1 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  0.600 J/cm²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 0.650 J/cm²
@Temperature 23.0 °C
3.09 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 100 µm/m-°C55.6 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 100 µm/m-°C55.6 µin/in-°FISO 11359-1/-2
Melting Point 178 °C352 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 163 °C325 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 108 °C226 °FISO 75-1/-2
Flammability, UL94  HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
IEC 60695-11-10
 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
IEC 60695-11-10
Flame Spread 25.0 mm/min
@Thickness 1.00 mm
0.984 in/min
@Thickness 0.0394 in
ISO 3795 (FMVSS 302)
 
Processing PropertiesMetricEnglishComments
Melt Temperature 195 - 205 °C383 - 401 °FExtrusion
 200 °C392 °FOptimum, Extrusion
 215 °C419 °FOptimum, Injection
 210 - 220 °C410 - 428 °FInjection
Mold Temperature 80.0 - 100 °C176 - 212 °FInjection
 90.0 °C194 °FOptimum, Injection
Drying Temperature  75.0 - 85.0 °C
@Time 7200 - 14400 sec
167 - 185 °F
@Time 2.00 - 4.00 hour
Extrusion; Dehumidified Dryer
 80.0 °C
@Time 7200 - 14400 sec
176 °F
@Time 2.00 - 4.00 hour
Injection; Dehumidified Dryer
Moisture Content 0.20 %0.20 %
Hold Pressure 80.0 - 100 MPa11600 - 14500 psiInjection
Annealing Temperature 160 °C320 °FOptional; 30 min/mm
 
Descriptive Properties
AdditivesLubricants
 Release agent
Delivery formPellets
Drying Recommendedyes
Emissions<8 mg/kgVDA 275
FMVSS ClassBISO 3795 (FMVSS 302)
Hold pressure time (s/mm)7.5Injection
Part Marking Code>POM<ISO 11469
ProcessingExtrusion
 Injection Molding
 Other Extrusion
 Sheet Extrusion
Regional AvailabilityAsia Pacific
 Europe
 Global
 Near East/Africa
 North America
 South and Central America
Resin IdentificationPOMISO 1043
UL 94 recognitionyes
 yes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDSX5155m / 254332

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.