MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Westlake EN923 Low Density Polyethylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Westlake Polyethylene EN923 is a low density formulation suggested for film applications where enhanced processability and high clarity are required. It is characterized by good tear strength, impact strength, a wide heat-sealing range and printability.

    Application/Uses
  • Food packaging
  • Household bags
  • Household wraps

FDA: This material complies with FDA regulations in 21 CFR, section 177.1520. Kosher Compliant.

All information provided by Westlake Chemical

Key Words: Enhanced processability and high clarity
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.920 g/cc0.0332 lb/in³ASTM D1505
Thickness 38.1 microns1.50 mil
Melt Flow 2.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.5 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 250 %250 %ASTM D882
Film Elongation at Break, TD 750 %750 %ASTM D882
Dart Drop 2.63 g/micron66.7 g/milASTM D1709
Film Tensile Strength at Break, MD 26.2 MPa3800 psiASTM D882
Film Tensile Strength at Break, TD 18.6 MPa2700 psiASTM D882
1% Secant Modulus, MD 186 MPa27000 psiASTM D882
1% Secant Modulus, TD 221 MPa32000 psiASTM D882
 
Optical PropertiesMetricEnglishComments
Haze 4.5 %4.5 %ASTM D1003
Gloss 75 %75 %at 45º; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Melt Temperature 182 - 193 °C360 - 380 °Fwith BUR of 2.4:1 or higher
Blow-up Ratio (BUR) 2.42.4
 
Descriptive Properties
ProcessFilm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mercury Gallium Sulfide, HgGa2S4
Greene Tweed CHEMRAZ® 584 Perfluoroelastomer
ASTM A285, Grade C
ASTM A283 Steel, grade C
304 Stainless Steel

PWESF094 / 84531

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.