MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Toyobo PELPRENE™ P40H-05 Polyester TPE, Non-smell, Non-deposit
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester TPE; Polyester, TP; Polyester Thermoplastic Elastomer

Material Notes: Features: Polyester TPE, Non-smell, Non-deposit

Information provided by Toyobo.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.12 g/ccASTM D792
Moisture Absorption at Equilibrium 0.48 %23°C, 65% RH
Linear Mold Shrinkage 0.0050 cm/cm
@Thickness 2.00 mm
Melt Index of Compound 10 g/10 min
@Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 89JIS K6301
Hardness, Shore D 38ASTM D2240
Tensile Strength at Break 23.0 MPaASTM D638
Elongation at Break 690 %ASTM D638
50% Modulus 0.00640 GPa
@Strain 50 %
ASTM D638
Flexural Modulus 0.0510 GPaASTM D790
Compressive Modulus 0.00450 GPa10%; ASTM D695
Resilience 78JIS K6301
Izod Impact, Notched NBASTM D256
Tear Strength 98.0 kN/mASTM D624
Taber Abrasion, mg/1000 Cycles 20ASTM D1044
Compression Set 50 %JIS K6301
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.00e+12 ohm-cmASTM D257
Dielectric Strength 20.0 kV/mmJIS K2111
 
Thermal PropertiesOriginal ValueComments
CTE, linear 170 µm/m-°C
@Temperature 20.0 °C
TMA
Melting Point 172 °CBy DSC
Vicat Softening Point 120 °CASTM D1525
Brittleness Temperature <= -65.0 °CJIS K6301
Flammability, UL94 HB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Envalior Arnitel® EM550 TPC-ET, Extrusion Grade
Toyobo PELPRENE™ P46D-01 Polyester TPE, High Viscous, High Durability
Envalior Arnitel® EM550 Polyether Ester Elastomer (European and Asian Grade)
Toyobo PELPRENE™ S2002 Polyester TPE, Ultra Heat-resistant
Toyobo PELPRENE™ S2001 Polyester TPE

PTOY679 / 70839

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.