MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials Kalrez® 9500 Fluoroelastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: DuPont™ Kalrez® 9500 perfluoroelastomer parts are a tan product for Deposition, Ash/Strip and Conductor (Poly/Metal) Etch processes. It has been specifically designed for use in applications where ozone is used for processing, e.g. SACVD, PECVD ultra-low K (BLOK™), and where the plasma environment is more “chemical”, i.e., where oxygen and fluorine radicals are more dominant. Kalrez® 9500 exhibits excellent resistance to CVD and ash/strip process chemistry, i.e., ozone, ammonia and water vapor. It also offers outstanding thermal stability, very low outgassing and excellent mechanical strength and is well suited for both static and dynamic sealing applications. A maximum continuous service temperature of 310 °C is suggested. Kalrez® 9500 can also withstand short-term excursions up to 325 °C. Ultrapure post-cleaning and packaging is standard for all Kalrez® 9500 parts.

Features/Benefits

  • Excellent resistance to CVD and ash/strip process chemistry (ozone, ammonia, water vapor, etc.)
  • Low erosion rate and ultra-low particle generation in radical dominant oxygen and fluorine-based plasmas
  • Excellent thermal stability
  • Very low outgassing and metals content
  • Excellent mechanical strength

Suggested Applications

  • Gas inlet/orifice/mixing block seals
  • Chamber lid seals
  • Isolation valve seals
  • Bonded gate valves/slit valve door seals

Information provided by DuPont

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.06 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 76ASTM D 2240
Elongation at Break 193 %ASTM D 412
100% Modulus 9.60 MPaASTM D 412
 
Thermal PropertiesOriginal ValueComments
CTE, linear 421 µm/m-°CISO 11359-1/-2
Maximum Service Temperature, Air 310 °CDuPont proprietary test
 
Descriptive Properties
ColorTan
Polymer(FFKM)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arlon Electronic Materials 33N Polyimide Laminate and Prepreg
3M Scotch-Weld™ DP820 Acrylic Adhesives
3M Scotch-Weld™ DP805 Acrylic Adhesives
3M Scotch-Weld™ DP270 Black Structural Adhesive
3M Scotch-Weld™ 826 Nitrile Rubber & Plastic Adhesive

PDVC9794 / 170435

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.