MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Northstar Polymers MSN-V40A Polyester Base Low-Rebound Impact/Vibration Dampening Gel
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced

Material Notes: This polyurethane casting material is developed for applications that require Shore OO 40 range casting material with vibration dampening property and higher strength than standard polyurethane gel material. The low tack surface of this material is also useful for application that does not use film/fabric encapsulation. At the elevated temperature, the component materials have lower viscosity for better flow in the mold for good resolution to reproduce fine mold surface or making thinner film/sheet material.

Processing this material requires elevated temperature process and constant agitation of part-B component. This material contains plasticizer. Plasticizer in general leaches out in a long term use of the product. This material is not recommended for applications that require cast-in encapsulation into plastic film material.

Information provided by Northstar Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore OO 4040
 
Processing PropertiesMetricEnglishComments
Processing Temperature 21.1 - 32.2 °C70.0 - 90.0 °FPrepolymer Temperature
 71.1 - 76.7 °C160 - 170 °FCuring Agent Temperature
Mold Temperature 82.2 °C180 °F
Cure Time  90.0 min
@Temperature 82.2 °C
1.50 hour
@Temperature 180 °F
De-mold Time
 480 - 960 min
@Temperature 71.1 - 82.2 °C
8.00 - 16.0 hour
@Temperature 160 - 180 °F
Complete Cure Cycle
Pot Life 7.00 - 9.00 min7.00 - 9.00 min
 
Descriptive Properties
Curing AgentSBX-146
PrepolymerMSA-018
Weight Ratio1:8.363Prepolymer to Curing Agent Ratio

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BCC Products BC 8782 Urethane Casting
Covestro Baytec® 33965-1 Polyurethane
Covestro Texin® 185 Urethane Thermoplastic Elastomer
Mearthane Durethane™ S DS-570D Solid Polyurethane Elastomer
Northstar Polymers MPP-V37A Polyurethane Gel Elastomer

PNORTH849 / 162565

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.