SMC LPMC 7680 is a sheet molding compound based on an unsaturated polyester resin, fire retardant grade, halogen-free, reinforced with glass fibers. SMC LPMC 7680 is studied to be molded at low pressure. This SMC has been developed for mass transportation. SMC LPMC 7680 joint good mechanical properties and high fire protection grade SMC LPMC 7680 complies with NF F 16-101. SMC LPMC 7680 is formulated according to RoHS, REAC regulation (SVHC) and WEEE European legislation.Information provided by Polynt Composites. |