Polyaryletherketone with carbon fibers, lubricant modified, dark grey Main features: Good friction and wear behavior especially at high temperatures. Electrically conductive, suitable for continuous discharging of statically-generated electricity. Information provided by Lehmann & Voss & Co.KG |