MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 1.0 PHR Sulfur
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced; Rubber or Thermoset Elastomer (TSE)

Material Notes: MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear strength, oil and fuel resistance, and ozone resistance. The life expectancy of urethane is often 5 times longer than other elastomers, thus saving material costs and downtime expense. One shortcoming of polyurethanes is loss of physical properties at temperatures over 180°F (82°C). MILLATHANE HT has overcome this weakness.

The sulfur-curing system consistently gives a desirable combination of optimum property values and processing safety. Selection of this system over peroxide, however, should be preceded by investigation into the possible effects of temperature. Sulfur-cured systems will give you better physical properties, but will not withstand a higher temperature of 300°F (149°C) as well as peroxidecured systems. A MILLATHANE HT masterbatch containing 40 phr N330 black was used in this evaluation.

All information provided by TSE Industries

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 80
Tensile Strength 2744 psi
Elongation at Break 433 %
100% Modulus 0.834 ksi
@Strain 100 %
200% Modulus 1.68 ksi
@Strain 200 %
300% Modulus 2.315 ksi
@Strain 300 %
Tear Strength 51.0 kN/mDie C
Compression Set 58 %
@Temperature 70.0 °C,
Time 79200 sec
 
Processing PropertiesOriginal ValueComments
Cure Time 12.0 min
@Temperature 160 °C
Press cured
 
Descriptive Properties
DIN Abrasion (mm³)129

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro DESMODUR® 0363 + BAYTEC® XL 0328 + BAYTEC® 0354 + BAYTEC® 0340 80A Polyurethane, MDI PPG
Covestro DESMODUR® MD15120-F + BAYTEC® D15-F + BAYTEC® XL B-F, 80A Polyurethane, MDI-Ester
Covestro DESMODUR® MD15120 +BAYTEC® D15 + BAYTEC® XL B, 80 A Polyurethane, MDI-Ester
Covestro DESMODUR®MD1578 + BAYTEC® D21 + BAYTEC® XL AL905 (Catalyst SD11-2) 80A Polyurethane, MDI-Ester
Covestro DESMODUR® TL535 + BAYTEC® XL 1705, 80 A Polyurethane, TDI- Caprolactone

PMILL252 / 87296

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.