MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Ultraform® W 2320 003 UNC Q600 POM
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: Ultraform W2320 003 UNC Q600 is a very easy flowing and rapidly solidifying injection molding POM grade for use where processing is extremely difficult but mechanical properties are lower. Contains a mold release agent. It conforms to FDA requirements of 21 CFR 177.2470.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.40 g/ccISO 1183
Water Absorption 0.80 %ISO 62
Moisture Absorption at Equilibrium 0.20 %23°C/50% R.H.; ISO 62
Melt Flow 29.4 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 145 MPaISO 2039-1
Tensile Strength, Yield 65.0 MPa50mm/min; ISO 527
Elongation at Break 24 %50mm/min; ISO 527
Elongation at Yield 7.5 %50mm/min; ISO 527
Modulus of Elasticity 2.80 GPaISO 527
Izod Impact, Notched (ISO) 5.00 kJ/m²
@Temperature 23.0 °C
ISO 180/A
 5.00 kJ/m²
@Temperature -30.0 °C
ISO 180/A
Charpy Impact Unnotched 15.0 J/cm²ISO 179
 15.0 J/cm²
@Temperature -30.0 °C
ISO 179
Charpy Impact, Notched 0.500 J/cm²ISO 179
 0.400 J/cm²
@Temperature -30.0 °C
ISO 179
Tensile Creep Modulus, 1 hour 2100 MPaISO 899
Tensile Creep Modulus, 1000 hours 1350 MPaISO 899
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohmIEC 60093
Dielectric Constant 3.8
@Frequency 100 Hz
IEC 60250
 3.8
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 40.0 kV/mmIEC 60243-1
Dissipation Factor 0.0010
@Frequency 100 Hz
IEC 60250
 0.0050
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 VTest Solution A; IEC 60112
 600 VTest Solution B; IEC 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 167 °CDIN 53765
Maximum Service Temperature, Air 100 °C
Deflection Temperature at 1.8 MPa (264 psi) 100 °CISO 75
Vicat Softening Point 150 °C(50 °C/h / 50N) - B/50; ISO 306
 
Processing PropertiesOriginal ValueComments
Melt Temperature 190 - 230 °C
Mold Temperature 60.0 - 120 °C
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
NSF YesNSF Std. 61
 
Descriptive Properties
ColorNatural
Commercial StatusActive America
Impact ModifiedNo
Primary Processing TechniqueInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultraform® N 2320 003 UNC Q600 POM
BASF Ultraform® W2320 003 PRO POM
BASF Ultraform® W 2320 003 BK120 Q600 POM
BASF Ultraform® W2320 U03 POM
BASF Ultraform® W2320 0035 POM

PBASF9113 / 84877

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.