MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SunChemical Gwent C70709D22 Silver Zinc Ink  (discontinued **)
Categories: Fluid; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: Silver Zinc Ink C70709D22 is designed as a screen printing ink for coating Barium Titanate PTC ceramics as the base layer of a two part system. The dried film should be coated with C70709D21 before final drying and firing.

The ink is in a ready to use form at a viscosity suitable for automatic or semiautomatic screen printing. The ink should be gently stirred before use avoiding introduction of air bubbles.

Information provided by Gwent Electronic Materials Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Particle Size 1.0 µm1.0 µmMain Break; Fineness of Grind
 3.0 µm3.0 µm3rd Streak; Fineness of Grind
Viscosity 14700 cP
@Shear Rate 230 1/s,
Temperature 25.0 °C
14700 cP
@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT550 cone and plate viscometer (PK1.1°)
Storage Temperature 20.0 °C68.0 °F
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 0.0071 ohm0.0071 ohmfired; 21 microns thick
 
Processing PropertiesMetricEnglishComments
Processing Temperature 150 °C302 °F
Cure Time 10.0 - 15 min0.167 - 0.25 hour
Shelf Life 3.00 Month3.00 Month
 
Descriptive Properties
Coverage cm2/g130230 mesh stainless steel screen
Printing Mesh counts/inch180 to 340stainless steel or polyester screens

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
American Elements Barium Titanate nanoparticles
Harris Acoustic Sensors EC-21 Barium Titanate Piezoelectric
Channel Industries 300 Barium Titanate Piezoelectric
Channel Industries 1300 Barium Titanate Piezoelectric
Barium Titanate, BaTiO3

WGEM099 / 75952

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.