MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Teijin Films Mylar® EC Polyester Film, 500 Gauge
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Mylar® EC films are electrical grade films designed for use in applications where improved dimensional stability is required. In addition to lower levels of shrinkage, Mylar® EC films offer outstanding durability, chemical inertness, good dielectrics, and good handling characteristics.

General Product Info: The outstanding strength, flexibility, and electrical properties of Mylar® EC films, combined with lower than normal shrinkage levels, make them especially suited for circuitry and membrane touch switch applications. The film's moisture and chemical resistance serve as a barrier to substances that could contaminate membrane touch switches.

Typical Applications: The unique balance of properties offered by Mylar® EC films makes them ideal for membrane switches and flexible circuits used in a variety of consumer and industrial products, including automotive instrument clusters, computers, calculators, telephones, cameras, and appliances.

Approvals: UL 94 VTM-2 - for 200 - 500 gauge (0.05 - 0.13mm)

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.3923 g/cc
Thickness 5.00 mil
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 160 %ASTM D882A
Film Elongation at Break, TD 160 %ASTM D882A
Film Tensile Strength at Break, MD 23000 psiASTM D882A
Film Tensile Strength at Break, TD 24000 psiASTM D882A
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 2700 V/mil1/4" electrode 500 V/sec 25°C in air; ASTM D149
Dielectric Breakdown 13500 V1/4" electrode 500 V/sec 25°C in air; ASTM D149
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 1.17 J/g-°CTypical Mylar®
Melting Point 254 °CTypical Mylar® via DSC
Shrinkage, MD 0.50 %
@Temperature 150 °C,
Time 1800 sec
Unrestrained
Shrinkage, TD 0.20 %
@Temperature 150 °C,
Time 1800 sec
Unrestrained
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.64 - 1.67typical of Mylar®
Optical Density 14[%]
Haze 31 %ASTM D1003
 
Descriptive Properties
Yield (nominal)4000 in2/lb

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Teijin Films Mylar® EC Polyester Film, 200 Gauge
DuPont Teijin Films Mylar® A Polyester Film, 900 Gauge
DuPont Teijin Films Melinex® 725 Polyester Film
DuPont Teijin Films Melinex® 329 Polyester Film, 500 Gauge
DuPont Teijin Films Melinex® 329 Polyester Film, 200 Gauge

PDTZ9317 / 139637

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.