MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Sipol Technipol® 157 Thermoplastic Adhesive Co-polyester
Categories: Polymer; Adhesive; Thermoplastic; Polyester, TP

Material Notes: Description: Technipol® 157 is a co-polyester based thermoplastic adhesive designed for the production of diesel filters in the automotive industry. Technipol® 157 is characterized by a high chemical resistance (mineral oil and diesel vapors) and by a good thermal resistance.

Information provided by SIPOL SpA

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.25 g/ccASTM D 792
Viscosity 18 cP
@Temperature 230 °C
 25 cP
@Temperature 210 °C
 30 cP
@Temperature 200 °C
 47 cP
@Temperature 180 °C
Brookfield Viscosity 37 cP
@Temperature 190 °C
Cone/ plate Viscometer, Model Brookfield CAP 2000+.; MI 12
Melt Flow 41 g/10 min
@Load 0.325 kg,
Temperature 190 °C
ASTM D 1238
Storage Temperature 5.00 - 10.0 °C
 
Mechanical PropertiesOriginal ValueComments
Elongation at Break >= 500 %ASTM D 638
 
Thermal PropertiesOriginal ValueComments
Melting Point 154 °CASTM D 3418
 
Processing PropertiesOriginal ValueComments
Processing Temperature 50.0 - 60.0 °CUnder Hopper
 120 - 160 °CCompression Zone
 170 - 180 °CMetering Zone
Feed Temperature 60.0 - 100 °C
Nozzle Temperature 170 - 180 °C
Die Temperature 170 - 180 °C
Shelf Life 12.0 Month
 
Descriptive Properties
Suggested temperature profile for melters165-175°CPre-Heating Grills
 180-190°CTank
 190-200°CHose
 190-200°CNozzle

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSIPOL005 / 297130

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.