MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Carmel Olefins Ipethene® 4140 LDPE Film Grade
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: IPETHENE® 4140 is a low-density polyethylene film grade, produced by high-pressure autoclave technology. Features: No additives, Good environmental stress, cracking resistance, Excellent bubble stability, Good mechanical properties. Uses: Large diameter agricultural films, Construction films, Shrink films, Pipes, Heavy duty bags. Processing Methods: Blown film extrusion, Blow molding.

Property data measured on samples of 100 µm blown film, Blow-up ratio 2.5:1, output 10 kg/h, melt temperature ~210°C.

Information provided by Carmel Olefins Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.920 g/cc0.0332 lb/in³ISO 1183-A
Thickness 100 microns3.94 milAs Tested
Melt Flow 0.13 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.13 g/10 min
@Load 4.76 lb,
Temperature 374 °F
1133
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 650 %
@Thickness 0.100 mm
650 %
@Thickness 0.00394 in
blown film; ISO 527-3
Film Elongation at Break, TD 700 %
@Thickness 0.100 mm
700 %
@Thickness 0.00394 in
blown film; ISO 527-3
Elmendorf Tear Strength MD 250 g
@Thickness 0.100 mm
250 g
@Thickness 0.00394 in
blown film; ISO 6383-2
Elmendorf Tear Strength TD 450 g
@Thickness 0.100 mm
450 g
@Thickness 0.00394 in
blown film; ISO 6383-2
Dart Drop Test 500 g
@Thickness 0.100 mm
1.10 lb
@Thickness 0.00394 in
F50. blown film; ISO 7765-A
Film Tensile Strength at Break, MD 24.0 MPa
@Thickness 0.100 mm
3480 psi
@Thickness 0.00394 in
blown film; ISO 527-3
Film Tensile Strength at Break, TD 27.0 MPa
@Thickness 0.100 mm
3920 psi
@Thickness 0.00394 in
blown film; ISO 527-3
 
Thermal PropertiesMetricEnglishComments
Melting Point 109 °C228 °FBy DSC; ISO 11357-3
Vicat Softening Point 97.0 °C
@Load 1.02 kg
207 °F
@Load 2.25 lb
ISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 210 °C410 °FAs Tested

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCARM825 / 249045

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.