System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Lucky CH-910 Acrylic, Coextrusion Grade
Categories:
Polymer
;
Thermoplastic
;
Acrylic (PMMA)
;
Acrylic, Extruded
Material Notes:
Coextrusion grade. May be UV stabilized. General Lucky PMMA qualities: Transparent/elegant appearance, high heat and weather resistance, excellent chemical resistance and coloring capability.
Key Words:
PMMA; Polymethylmethacrylate; Polymethyl Methacrylate
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.18
g/cc
ASTM D792
Linear Mold Shrinkage
0.0020
-
0.0060
cm/cm
ASTM D955-51
Melt Flow
1.0
g/10 min
ASTM D1238
Mechanical Properties
Original Value
Comments
Hardness, Rockwell M
97
ASTM D785
Tensile Strength, Ultimate
74.0
MPa
ASTM D638
Elongation at Break
3.5 %
ASTM D638
Flexural Yield Strength
135
MPa
ASTM D790
Flexural Modulus
3.30
GPa
ASTM D790
Electrical Properties
Original Value
Comments
Dielectric Strength
20.0
kV/mm
ASTM D149
Thermal Properties
Original Value
Comments
Maximum Service Temperature, Air
98.0
°C
Heat Distortion Temp
98.0
°C
Deflection Temp; Load not reported; ASTM D648
Vicat Softening Point
105
°C
ASTM D1525
Optical Properties
Original Value
Comments
Refractive Index
1.49
ASTM D542
Transmission, Visible
92 %
ASTM D1003
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Lucky IF-850 Acrylic, Injection Grade
Arkema Altuglas® 84 L Acrylic-Styrene Copolymer
Lucky CF-920 Acrylic
Lucky CG-920 Acrylic
Lucky EF-940 Acrylic, Injection/Extrusion Grade
PLAL08 / 49859
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.