MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NIZHNEKAMSKNEFTEKHIM PE 4052V (52418) High Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.

Information provided by manufacturer

Key Words: PE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.950 - 0.954 g/ccBase Resin; ASTM D1505
Melt Flow 16 - 20 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1283/L
 480 - 600 g/10 min
@Load 21.6 kg,
Temperature 190 °C
Flow@21.6kg/Flow@2.16kg ratio < 30; ASTM D1283
 
Mechanical PropertiesOriginal ValueComments
Flexural Modulus >= 1250 MPaASTM D790
Izod Impact, Notched >= 40.0 J/m
@Temperature 23.0 °C
ASTM D256

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NIZHNEKAMSKNEFTEKHIM PE 2062U (62111) High Density Polyethylene
NIZHNEKAMSKNEFTEKHIM PE 2060V (60118) High Density Polyethylene
NIZHNEKAMSKNEFTEKHIM PE 2062T (62107) High Density Polyethylene
NIZHNEKAMSKNEFTEKHIM PE 2062x (62135) High Density Polyethylene
NIZHNEKAMSKNEFTEKHIM PE 4050Q (50403) High Density Polyethylene

PNKNH086 / 109353

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.