MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Paratherm Corporation Paratherm™ HT Heat Transfer Fluid
Categories: Fluid

Material Notes: Paratherm HT Heat Transfer Fluid is a partially hydrogenated terphenyl based product designed for closed-loop liquid phase heating to 650°F (343°C) in fired heaters and 675°F (358°C) in solid fuel-fired heat recovery and full convection heaters. Applications include:gas processing, chemical processes, waste oil recovery, biodiesel production, and plastic processing.

Information provided by Paratherm Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.34 lb/gal
@Temperature 23.9 °C
 8.40 lb/gal
@Temperature 15.6 °C
Viscosity Measure 0.54 cSt
@Temperature 343 °C
 4.2 cSt
@Temperature 100 °C
 31 cSt
@Temperature 40.0 °C
Molecular Weight 330 g/molaverage; ASTM D2502
Vapor Pressure 0.7830 atm
@Temperature 357 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 167 µin/in-°F
@Temperature 20.0 - 75.6 °C
Boiling Point >= 349 °C
@Pressure 0.101 MPa
ASTM D1160
Maximum Service Temperature, Air 650 °Ffired heaters
 675 °Fall except fired heaters
 700 °Fmax. recommended film temperature
Minimum Service Temperature, Air 124 °F20 cPs
Flash Point >= 340 °Fpmcc - Pensky-Martens Closed Cup; ASTM D93
 
Descriptive Properties
Appearancepale yellow
Odormild

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum 5083-H116; 5083-H321
304 Stainless Steel (UNS S30400); Hot Finished and Annealed Bar and Forgings
Uninhibited Naval brass, UNS C46400, M20 Temper 25 mm flat products
ThyssenKrupp COR-TEN A Structural Steel
Paratherm Corporation Paratherm™ HR™ Heat Transfer Fluid

WPAR04m / 176007

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.