Hifax polypropylene resins based on the Catalloy process are used in applications such as building and construction (e.g., single-ply roofing), industrial applications (e.g., wire and cable), and automotive industries. Hifax priovides good processability, excellent impact resistance, a broad range of stiffness from very soft to rigid products, high temperature resistance and low linear coefficient of thermal expansion. Hifax TRS 372P is an unfilled PP copolymer, with excellent processability, excellent impact resistance and good UV resistance. Applications: Automotive Parts, Exterior Automotive Applications. Information provided by LyondellBasell. |