MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Flame Retardant adhesives

Sumitomo Bakelite SUMILITE® EL-3700 Epoxy Laminate
Categories: Polymer; Thermoset; Epoxy; Epoxy/Glass SMC

Material Notes: Unclad glass epoxy lamnetes for polishing & lapping carrier

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Absorption 0.080 %0.080 %E-24/50+D-24/23
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 110110
Flexural Strength 540 MPa78300 psiWidthwise
 650 MPa94300 psiLengthwise
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 V-0V-0Flame Retardancy; F-168/70
 
Descriptive Properties
ColorNatural
Insulation Resistance200000000000Ohm; A
 90000000000Ohm; D-2/100

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Bakelite® EP 8412 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage
Norplex-Micarta NP500A Epoxy Glass Laminate Sheet, NEMA G-10
Sumitomo Bakelite Durez® 118 Phenolic, Injection Grade
Sumitomo Bakelite SUMILITE® EL-3700M Epoxy Laminate
Sumitomo Bakelite SUMILITE® EL-3762 Glass Epoxy Laminate

PSUMIT101 / 193906

Flame Retardant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.