MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Trinseo CALIBRE™ 603-3 Polycarbonate, Branched
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Unreinforced, Flame Retardant

Material Notes: CALIBRE™ 603-3 is a branched polycarbonate resin specially designed for extrusion of profiles, corrugated sheet and very complex multi-wall sheet. CALIBRE™ 603-3 offers a very high melt strength to calibrate effectively the most complex multi-wall sheet structures, such as a seven wall sheet or more, and to calibrate effectively complex profiles and corrugated sheet. CALIBRE™ 603-3 contains a UV absorber additive, but note that sheets for outdoor applications also require a protective UV-absorption cap layer. It is recommended to coextrude a 50 µm thick cap layer, using CALIBRE™ 320UV.

Main Characteristics:

  • Very high melt strength
  • Good impact resistance
Application:
  • Complex multi-wall sheet
  • ProfilesData provided by Dow Chemical.

Key Words: PC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccISO 1183/B
Water Absorption 0.15 %24 hr; ISO 62
Moisture Absorption at Equilibrium 0.32 %50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cmISO 294-4
Melt Flow 3.0 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 66.0 MPaISO 527-2/50
Tensile Strength, Yield 62.0 MPaISO 527-2/50
Elongation at Break 100 %ISO 527-2/50
Elongation at Yield 6.0 %ISO 527-2/50
Tensile Modulus 2.30 GPaISO 527-2/50
Flexural Strength 94.0 MPa2 mm/min; ISO 178
Flexural Modulus 2.30 GPa2 mm/min; ISO 178
Izod Impact, Notched (ISO) 15.0 kJ/m²
@Temperature -30.0 °C
ISO 180/A
 80.0 kJ/m²
@Temperature 23.0 °C
ISO 180/A
Charpy Impact, Notched 1.60 J/cm²
@Temperature -30.0 °C
ISO 179/1eA
 5.50 J/cm²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 250 V
@Thickness 2.00 mm
Solution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 39.0 µm/m-°CISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 145 °CAannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 126 °CUnannealed; ISO 75-2/A
 142 °CAannealed; ISO 75-2/A
Vicat Softening Point 150 °CISO 306/B50
Flammability, UL94 HB
@Thickness 1.50 mm
 HB
@Thickness 3.05 mm
Glow Wire Flammability Index 775 °C
@Thickness 1.02 mm
Ignition Temperature; IEC 60695-2-13
 775 °C
@Thickness 2.03 mm
Ignition Temperature; IEC 60695-2-13
 775 °C
@Thickness 3.05 mm
Ignition Temperature; IEC 60695-2-13
 875 °C
@Thickness 2.03 mm
Flammability Index; IEC 60695-2-12
 875 °C
@Thickness 3.05 mm
Flammability Index; IEC 60695-2-12
 900 °C
@Thickness 1.02 mm
Flammability Index; IEC 60695-2-12
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.586ISO 489
Haze 1.0 %ASTM D1003
Transmission, Visible 89 %ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Samyang Trirex® PC-3027U 6 MFI UV Stabilized Clear Polycarbonate
SABIC Lexan® 131R PC (Asia Pacific)
Covestro Makrolon® ET3227 Polycarbonate
Covestro Makrolon® WB1239 Polycarbonate
LG Chemical IH830 PMMA, General Purpose Grade for Injection Molding

PZZDW030 / 34261

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.