MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Kazanorgsintez OS-20 Textile Auxiliary Agent
Categories: Fluid; Solvent

Material Notes: Production Method: Obtained by interaction of higher synthetic fatty alcohols with ethylene oxide.

Application: Grade A is used in the chemical industry as a surface-active materialtant. Grade B is used in the textile industry as an antistatic agent and as a leveling agent in the painting process.

Information Provided by Kazanorgsintez

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
pH 8.0 - 10.5pH value of aqueous solution with OS-20 mass fraction of 10%, Highest Quality and 1st Quality
Ash <= 0.20 %
 
Optical PropertiesOriginal ValueComments
Optical Density 0.40Optical density of aqueous solution with OS-20 mass fraction of 10%
 
Component Elements PropertiesOriginal ValueComments
Iron, Fe <= 0.0020 %
 <= 0.0030 %
 
Descriptive Properties
AppearanceAt room temperature:

Grade A: Waxy scales of white to yellow color

Grade B: Waxy solid mass, from yellow to light-brown color.

Cloud Point of Os-20; 1% in Sodium Chloride Solution; Base Substance of 5% (°C)86-961st Quality
 90-96Highest Quality
Color6Melt chromaticity by Iodine scale, mg of J2 per 100 cm3
Hydroxyl Number, mg of KOH/g of PEG-41st Quality
 Highest Quality

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PKAZAN130 / 127449

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.