MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Parson Adhesives PARFIX® 3430 Cyanoacrylate Adhesive
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: PARFIX 3430 is medium viscosity combined with fast cure speed, metal bonding Cyanoacrylate adhesive (CA). It is specifically formulated to bond various metals such as Aluminum, Stainless Steel, Copper, etc.

Applications:

  • Ideal for bonding Metal Surfaces to itself and to Wood, Balsa Wood, Rubber, Plastics, Leather, etc.
  • Wiper blades, Nameplates, Gearshift indicators, aerospace parts, automotive parts, Machinery parts, Electronic components, Transportation equipment, etc.
  • Ideal for wide variety of metal bonding and fixing applications.
  • Meets MLLA 46050 Type I class II specifications requirement

Information provided by Parson Adhesives, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Shear Strength >= 5.00 MPa>= 725 psiABS; ASTM D1002
 >= 10.0 MPa>= 1450 psiPolycarbonate; ASTM D1002
 >= 13.0 MPa>= 1890 psiCopper; ASTM D1002
 13.0 - 20.0 MPa1890 - 2900 psi
 >= 20.0 MPa>= 2900 psiGrit Blasted Steel; ASTM D1002
 >= 20.0 MPa>= 2900 psiEtched Aluminum; ASTM D1002
 >= 20.0 MPa>= 2900 psiStainless Steel; ASTM D1002
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D696
Dielectric Constant 2.32.3ASTM D150
Dielectric Strength 0.984 kV/mm25.0 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear 100 µm/m-°C55.6 µin/in-°FASTM D696
Thermal Conductivity 0.100 W/m-K0.694 BTU-in/hr-ft²-°FASTM C177
Melting Point 160 - 170 °C320 - 338 °F
Maximum Service Temperature, Air 80.0 °C176 °F
Minimum Service Temperature, Air -51.1 °C-60.0 °F
Glass Transition Temp, Tg 120 °C248 °FASTM E228
 
Processing PropertiesMetricEnglishComments
Cure Time 0.0500 - 0.167 min0.000833 - 0.00278 hourPVC/PVC, Fixture
 0.167 - 0.250 min0.00278 - 0.00417 hourSBR/SBR, Fixture
 0.167 - 0.330 min0.00278 - 0.00550 hourCopper/Copper, Fixture
 0.250 - 0.330 min0.00417 - 0.00550 hourSteel/PVC, Fixture
 0.167 - 0.500 min0.00278 - 0.00833 hourSteel/Steel, Fixture
 0.167 - 1.00 min0.00278 - 0.0167 hourAluminum/Aluminum, Fixture
 0.500 - 1.00 min0.00833 - 0.0167 hourStainless Steel/Stainless Steel, Fixture
 1440 min24.0 hourFull
 
Descriptive Properties
AppearanceColorless Liquid
CompositionMethyl Cyanoacrylate
Gap Filling0.20 mm
Initial Strength Retained (%)75Gasoline for 1000 hrs at 22°C
 80Gasoline for 500 hrs at 22°C
 85Isopropanol for 500 hrs at 22°C
 85Isopropanol for 1000 hrs at 22°C
 90Motor Oil for 500 hrs at 40°C
 90Motor Oil for 1000 hrs at 40°C
 90Mineral Spirit for 500 hrs at 22°C
 90Mineral Spirit for 1000 hrs at 22°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sandvik Manganin® 43 Resistance Wire
Composition Spec for Aluminum 343.1

PPARSN130 / 186573

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.