MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

CMW® 3000 AMS-T-21014 AMS-7725 High Density Machinable Tungsten  (discontinued **)
Categories: Metal; Nonferrous Metal; Refractory Metal; Tungsten Alloy

Material Notes: This material has been rebranded as NAECOMET® 3000.

Uses: Radiation Shielding, High Mass, Gyro, Ordnance. Machinability is similar to gray iron.

Information provided by CMW Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 17.24 g/cc0.6228 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell A 63
@Temperature 600 °C
63
@Temperature 1110 °F
32 HRA
Hardness, Rockwell C 2525
Tensile Strength, Ultimate 862 MPa125000 psi
Tensile Strength, Yield 607 MPa88000 psi
Elongation at Break 18 %18 %
Modulus of Elasticity 352 GPa51100 ksi
Compressive Yield Strength 603 MPa87500 psi
Fatigue Strength 427 MPa61900 psiHigh cycle unnotched
Charpy Impact 9.50 J7.01 ft-lbNotched
Charpy Impact, Unnotched 203 J150 ft-lb
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00001724 ohm-cm0.00001724 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear  4.61 µm/m-°C
@Temperature 20.0 - 400 °C
2.56 µin/in-°F
@Temperature 68.0 - 752 °F
 5.36 µm/m-°C
@Temperature 20.0 - 800 °C
2.98 µin/in-°F
@Temperature 68.0 - 1470 °F
Thermal Conductivity 75.7 W/m-K525 BTU-in/hr-ft²-°F
Melting Point 1425 - 3410 °C2597 - 6170 °F
Solidus 1425 °C2597 °F
Liquidus 3410 °C6170 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 3.0 %3.0 %
Nickel, Ni 7.0 %7.0 %
Tungsten, W 90 %90 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CMW® 2000 AMS-T-21014 ASTM B777 High Density Machinable Tungsten
Astaras ANVILOY® 1150 Tungsten Based High Temp Alloy
Arc Cast Molybdenum TZM (Mo-0.5Ti-0.1Zr; Mo alloy 363), Stress Relieved
NAECO® NAECOMET® 2000 AMS-T-21014 ASTM B777 High Density Machinable Tungsten
Molybdenum TZC (Mo-1Ti-0.3Zr)

NCMW05 / 15876

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.