Fast crystallization. Suitable for higher viscosity adhesives than those made with DCR-15L Chloroprene rubber (CR) is a synthetic rubber possessing excellent mechanical strength, flame resistance, and adhesive strength, coupled with a well-balanced combination of weather ability and resistance to ozone, heat, and oil. CR is widely used in industrial products, cables, adhesives, etc. Chloroprene rubber demonstrates a good balance of features, including such as resistance to ozone, oil and heat, flame retardant, weather ability, special cohesiveness, etc, and is very easy to process. Uses: Electrical wiring and cables, Automotive components, Coated cloth, form rubber, General industrial articles, Adhesives, etc. Information provided by Denka Company Limited. |