MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
MRC Polymers MAXNITE™ 500 GF15 PET, 15% Glass Fiber Filled  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), 20% Glass Reinforced

Material Notes:

Information provided by MRC Polymers Inc.

Key Words: PET
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.43 g/ccASTM D792
Filler Content 15 %+/- 2%; ASTM D2584
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 12000 psiASTM D638
Elongation at Break 2.0 %ASTM D638
Flexural Strength 19.0 ksiASTM D790
Flexural Modulus 850 ksiASTM D790
Izod Impact, Notched 1.20 ft-lb/in
@Temperature 22.8 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 410 °FASTM D648
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 500 - 540 °F
Middle Barrel Temperature 500 - 550 °F
Front Barrel Temperature 510 - 550 °F
Nozzle Temperature 520 - 570 °Freverse tapered recommended
Melt Temperature 520 - 560 °F
Mold Temperature 180 - 220 °Fthick wall - thin wall
Drying Temperature 240 - 275 °F
Dry Time 4 - 6 hour
Moisture Content <= 0.020 %
Dew Point <= 0.000 °F
Drying Air Flow Rate 0.800 - 1.00 ft³/min (CFM)per lb/hour resin processed
Injection Pressure 10000 - 20000 psi
Back Pressure 50.0 - 175 psikeep minimum
Cushion 0.250 in
Screw Speed 20 - 50 rpm
 
Descriptive Properties
DryerDehumidified hopper
Fill RateModerate-Fast
Hold Pressure40-60% of injection pressure
Packing Pressure50-75% of injection pressure

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Celcon® LU-02 POM, UV Resistant
Bisalloy Steels BisPlate 80PV Thickness 6-<16 mm
Ineos Nova Zyntar® 779 High Performance Flame Retardant Polystyrene
UCAR Carbon UCAR® PGW Pressure Molded Graphite
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced

PMRC009 / 89438

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.