MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SunChemical Gwent C2050303D1 Fine Line Silver Printing Ink
Categories: Fluid; Metal; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: Silver Ink has been designed for fine line printing. It is capable of printing down to 50 micron line and spaces within a production environment. Under laboratory conditions, finer lines and spaces have been produced. The ink has been made at a ready to use viscosity and should be thoroughly stirred before use avoiding introduction of air bubbles. It can be printed on automatic and semi automatic screen printers.
Screen Printing Equipment: semi-automatic, automatic
Screen Types: stainless steel, polyester, mesh 156-325 tpi
Substrate: Polyester, PVC, Polycarbonate or ceramic

Information provided by Gwent Electronic Materials Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 69 - 71 %
@Temperature 700 °C
69 - 71 %
@Temperature 1290 °F
Viscosity 14000 - 16000 cP
@Shear Rate 230 1/s,
Temperature 25.0 °C
14000 - 16000 cP
@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Storage Temperature 20.0 °C68.0 °Fsealed container
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 0.0021 ohm
@Treatment Temp. 850 °C,
Thickness 0.0180 mm
0.0021 ohm
@Treatment Temp. 1560 °F,
Thickness 0.000709 in
 
Processing PropertiesMetricEnglishComments
Sintering Temperature >= 700 °C>= 1290 °F
Cure Time  10.0 min
@Temperature 150 °C
0.167 hour
@Temperature 302 °F
 15.0 min
@Temperature 120 °C
0.250 hour
@Temperature 248 °F
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
Coverage cm2/g80Using a 230 mesh stainless steel screen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Molybdenum, Mo, Annealed
Lanxess LEWATIT® Regler ZL Ion Exchange Resin

WGELZ9080 / 139393

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.