MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Momentive Performance Materials GE Silicones RCS20 All-purpose siliconized acrylic latex gun grade sealant
Categories: Polymer; Thermoset; Silicone

Material Notes: RCS20 siliconized acrylic sealant is a premium quality, all-purpose siliconized acrylic latex gun grade sealant that can be used for interior and exterior caulking and sealing. It provides excellent adhesion to most construction surfaces with superior flexibility and is an excellent candidate for use in sealing seams, cracks and joints around doors, windows, woodwork, siding, flashing, air conditioners, baseboards and countertops. RCS20 siliconized acrylic sealant may be suitable for use as an acoustical sealant for reducing sound transmission in a wall system.

Features: Excellent Adhesion, Superior Flexibility, Acoustical Performance, Paintable, Trouble Free Installation, Long-Term Service, Stable Consistency, Non-Staining, Clean, Industry Standards, Versatility with GE Acrylic Products, Easy Clean-Up.

Applications: RCS20 siliconized acrylic sealant is designed to provide water and weather protection by forming an airtight seal when used on interior and exterior surfaces. Can be used for caulking window and door frames, vinyl, steel, aluminum, plywood siding, drywall, baseboards, bathroom & kitchen fixtures, primed fiber cement siding and conventional stucco. RCS20 siliconized acrylic sealant can be used to patch non-structural cracks and joints on many common substrates, including: stucco, precast concrete, concrete block, brick and wood. RCS20 siliconized acrylic sealant is useful as an acoustical sealant in the construction of walls, windows, doors, ceilings and floors to reduce sound transmission in wall partitions to maintain specified STC and OITC values. Use it to seal all adjacent similar or dissimilar materials on both sides of partitions and walls, around electrical box cutouts, under tracks and around door frames and window perimeters.

Information provided by Momentive Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.61 g/ccLab Value
Solids Content 69.45 - 71.45 %
 80 - 84 %
Volatile Organic Compounds (VOC) Content 53.4 g/lCalculated
pH 7.7 - 8.1
 
Mechanical PropertiesOriginal ValueComments
Elongation at Break 325 %ASTM D-412
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 180 °F
Minimum Service Temperature, Air -10.0 °F
 
Processing PropertiesOriginal ValueComments
Dry Time 24.0 hour
@Temperature 23.9 °C
To cure
Extrusion Rate 2820 g/min
@Temperature 25.0 °C
ASTM C-731
Shelf Life >= 12.0 MonthLab value
 
Descriptive Properties
AppearanceSmoothCured
 Thixotropic, heavy bodied.
ColorTranslucentRCS20.01
 WhiteRCS20.02
Coverage Rate50 linear feetAt 3/16" bead.
Crack ResistancePass(unpainted)Wood Channel 1/2” x 1/2”
FlexibilityPass90° @ -18°C (1/8" slab). 1" Mandrel on Aluminum.
Freeze/Thaw Stability5 cycles
OdorSlight Ammonia Odor
Prime PigmentRutile Titanum Dioxide
SlumpNoneASTM D-2202
VehicleAcrylic Terpolymer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMOMEN9931 / 265742

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.